X50CrMoV15

Martensitic stainless steel, excellent for cutting tools.

Equivalent: Aisi Stainless 440C

W.1.4116

C Cr Mo V
0.48-0.60   14.50  0.65  0.15  

 

 

HEAT TREATMENT: Hardening temperature 980-1050°C (1795 - 1925°F), holding time 5 minutes, Quenching in oil.

Tempering 2 hours

160 celsius .........58-58,5 hrc

 